ABSTRACT:
Low gloss appearance in a coating derived from UV curable powder coatings can be achieved by using UV curable powder containing crystalline resins or blends of crystalline and amorphous resins and after heat fusing the powders together, allowing the crystalline resins in the coating to cool and recrystallize to a low gloss finish before curing with UV radiation.
REFERENCES:
K.M. Biller, et al., UV Curable Powders: A Marriage of Compliant Coatings,Indus. Paint & Powder, Jul. 1996, 22-25.
K.M. Biller, et al.,UV Curable Powder Coatings, Proceedings from RadTech 96 Conference. Apr.1996, pp. 437-445.
D.S. Richart, Powder Coatings Clinic, Powder Coating, Apr. 1996, pp. 55-56.
Daly Andrew T.
Haley Richard P.
Mill Gregory R.
Reinheimer Eugene P.
Benjamin Steven C.
Morton International Inc.
Parker Fred J.
White Gerald K.
LandOfFree
Method for producing low gloss appearance with UV curable powder does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for producing low gloss appearance with UV curable powder, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for producing low gloss appearance with UV curable powder will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2314289