ABSTRACT:
The invention relates to a method for producing lithium-transition metal mixtures of general formula Lix(M1yM21-y)nOnz, wherein M1represents nickel, cobalt or manganese, M2represents chromium, cobalt, iron, manganese, molybdenum or aluminium, and is different from M1, n is 2 if M1represents manganese and is 1 otherwise, x is comprised between 0.9 and 1.2, y is comprised between 0.5 and 1.0 and z is comprised between 1.9 and 2.1. According to the inventive method, an intimate mixture composed of transition metal compounds containing oxygen and of a lithium compound containing oxygen is calcinated, said mixture being obtained by processing a solid powder transition metal compound with a solution of said lithium compound, and then drying. At least the M1compound is used in powder form having a specific surface of at least 20 m2/g (BET) and calcination is carried out in a fluidised bed.

REFERENCES:
patent: 4567031 (1986-01-01), Riley
patent: 4668595 (1987-05-01), Yoshino et al.
patent: 4770960 (1988-09-01), Nagaura et al.
patent: 4980080 (1990-12-01), Lecerf et al.
patent: 5180574 (1993-01-01), Von Sacken
patent: 5264201 (1993-11-01), Dahn et al.
patent: 5391265 (1995-02-01), Krynitz et al.
patent: RE34991 (1995-07-01), Yoshino et al.
patent: 5591548 (1997-01-01), Mao
patent: 5629110 (1997-05-01), Kobayashi et al.
patent: 5702679 (1997-12-01), Sheargold et al.
patent: 5720932 (1998-02-01), Amine et al.
patent: 5728367 (1998-03-01), Mao
patent: 1102909 (1995-05-01), None
patent: 0643430 (1995-03-01), None
patent: 0643430 (1995-03-01), None
patent: 0806397 (1997-11-01), None
patent: 0806397 (1997-11-01), None
patent: 2704216 (1994-10-01), None
patent: WO9425398 (1994-11-01), None
patent: 7-105950 (1995-04-01), None
patent: 10-152327 (1998-06-01), None
patent: WO 9425398 (1994-11-01), None
Journal of Power Sources 54 (month unavailable) 1995, pp. 209-223, Shuji Yamada et al, “Synthesis and properties of LiNiO2as cathode material for secondary batteries”.
Journal of Power Sources 54 (month unavailable) 1995, pp. 329-333, R.V. Moshtev et al, “The LiNiO2solid solution as a cathode material for rechargeable lithium batteries”.
Journal of Power Sources 54 (month unavailable) 1995, pp. 522-524, T. Nohma et al, “Electrochemical characteristics of LiNiO2and LiCoO2as a positive material for lithium secondary batteries”.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for producing lithium-transition metal mixtures does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for producing lithium-transition metal mixtures, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for producing lithium-transition metal mixtures will most certainly appreciate the feedback.