ABSTRACT:
The high carbon steel wire rod contains 0.65% to 1.20% of C, 0.05% to 1.2% of Si, 0.2% to 1.0% of Mn, and 0.35% or less (including 0%) of Cr, further contains P and S each in an amount restricted to 0.02% or less, where 80% or more of the metal structure is constituted by a pearlite structure; and an average tensile strength TS and an average lamellar spacing λ of the high carbon steel wire rod show the relation of TS≦8700/√{square root over ( )}(λ/Ceq)+290 in which Ceq=% C+% Mn/5+% Cr/4. The high carbon steel wire rod can omit a patenting treatment before or during wire drawing, is superior in wire drawability, and exhibits a low drawing resistance in a wire drawing die in an as-hot-rolled state.

REFERENCES:
patent: 5776267 (1998-07-01), Nanba et al.
patent: 6322641 (2001-11-01), Makii et al.
patent: 6645319 (2003-11-01), Nagao et al.
patent: 6783609 (2004-08-01), Hata et al.
patent: 6800147 (2004-10-01), Nagao et al.
patent: 2004/0129354 (2004-07-01), Nagao et al.
patent: 2005/0155672 (2005-07-01), Nagao
patent: 0 624 658 (1994-11-01), None
patent: 1 277 846 (2003-01-01), None
patent: 3-60900 (1991-09-01), None
patent: 4-346618 (1992-12-01), None
patent: 6-346190 (1994-12-01), None
patent: 11-302743 (1999-11-01), None
patent: 11-315348 (1999-11-01), None
patent: 2000-63987 (2000-02-01), None
patent: 2001-179325 (2001-07-01), None
patent: 2004-137597 (2004-05-01), None
patent: 2004-149816 (2004-05-01), None
patent: 2004-288589 (2004-10-01), None
patent: 2001-0008462 (2001-02-01), None
patent: WO 2004/029315 (2004-04-01), None
U.S. Appl. No. 11/022,792, filed Dec. 28, 2004, Nagao.
U.S. Appl. No. 10/968,253, filed Oct. 20, 2004, Nagao et al.
U.S. Appl. No. 10/528,263, filed Mar. 17, 2005, Nagao et al.
U.S. Appl. No. 11/296,299, filed Dec. 8, 2005, Minamida et al.
Patent Abstracts of Japan, JP 2000-063987, Feb. 29, 2000.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for producing high carbon steel wire rod superior in... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for producing high carbon steel wire rod superior in..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for producing high carbon steel wire rod superior in... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3925357

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.