Method for producing a titanium-base alloy having an oxide...

Powder metallurgy processes – Powder metallurgy processes with heating or sintering – Metal and nonmetal in final product

Reexamination Certificate

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C419S020000, C419S030000

Reexamination Certificate

active

07037463

ABSTRACT:
A metallic article is prepared by first furnishing at least one nonmetallic precursor compound, wherein all of the nonmetallic precursor compounds collectively containing the constituent elements of the metallic article in their respective constituent-element proportions. The constituent elements together form a titanium-base alloy having a stable-oxide-forming additive element therein, such as magnesium, calcium, scandium, yttrium, lanthanum, cerium, praseodymium, neodymium, promethium, samarium, europium, gadolinium, terbium, dysprosium, holmium, erbium, thulium, ytterbium, and lutetium, and mixtures thereof. The stable-oxide-forming additive element forms a stable oxide in a titanium-based alloy. At least one additive element is present at a level greater than its room-temperature solid solubility limit in the titanium-base alloy. The precursor compounds are chemically reduced to produce an alloy material, without melting the alloy material. The alloy material may be consolidated. The alloy material, or consolidated metallic article, is thereafter desirably exposed to an oxygen-containing environment at a temperature greater than room temperature.

REFERENCES:
patent: 4512826 (1985-04-01), Whang
patent: 4622079 (1986-11-01), Chang et al.
patent: 4731111 (1988-03-01), Kopatz et al.
patent: 4906436 (1990-03-01), Gigliotti et al.
patent: 4915905 (1990-04-01), Kampe et al.
patent: 4999336 (1991-03-01), Nadkarni et al.
patent: 5041262 (1991-08-01), Gigliotti, Jr.
patent: 5322666 (1994-06-01), Watwe
patent: 5431874 (1995-07-01), Gigliotti, Jr.
patent: 5779761 (1998-07-01), Armstrong et al.
patent: 5830288 (1998-11-01), Gigliotti et al.
patent: 5930580 (1999-07-01), Everett
patent: 5958106 (1999-09-01), Armstrong et al.
patent: 6019812 (2000-02-01), Volas et al.
patent: 6264719 (2001-07-01), Zhang et al.
patent: 6737017 (2004-05-01), Woodfield et al.
patent: WO 99/64638 (1999-12-01), None
patent: WO 9964638 (1999-12-01), None

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for producing a titanium-base alloy having an oxide... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for producing a titanium-base alloy having an oxide..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for producing a titanium-base alloy having an oxide... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3578880

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.