ABSTRACT:
A method for producing a silicon nitride filter, which comprises heat-treating in nitrogen a green body comprising from 60 to 95 mass % of metal silicon particles having an average particle diameter of from 10 to 75 μm, wherein particles having particle diameters of from 5 to 100 μm are at least 70 mass % in the entire metal silicon particles, and from 5 to 40 mass % of a pore-forming agent, to convert metal silicon substantially to silicon nitride. More preferably, the green body contains at least one member selected from the group consisting of an inorganic acid salt, an organic acid salt and a hydroxide containing at least one metal element selected from the group consisting of Mg, Ca, Fe and Cu.

REFERENCES:
patent: 3960581 (1976-06-01), Cutler
patent: 6565797 (2003-05-01), Miyakawa et al.
patent: 6593261 (2003-07-01), Shinohara et al.
patent: 6849213 (2005-02-01), Miyakawa et al.
patent: 6869902 (2005-03-01), Inoue et al.
patent: 7135140 (2006-11-01), Shinohara et al.
patent: 2005/0023735 (2005-02-01), Miyakawa et al.
patent: 1 160 223 (2001-12-01), None
patent: 1 197 253 (2002-04-01), None
patent: 1 426 216 (1976-02-01), None
patent: 1546928 (1979-05-01), None
patent: 52-121613 (1977-10-01), None
patent: 6-256069 (1994-09-01), None
patent: 7-187845 (1995-07-01), None
patent: 8-59364 (1996-03-01), None
patent: 2002-284585 (2002-10-01), None
patent: WO 01/47833 (2001-07-01), None
patent: WO 2004/050318 (2004-06-01), None
U.S. Appl. No. 11/240,509, filed Oct. 3, 2005, Shinohara et al.
U.S. Appl. No. 11/287,461, filed Nov. 28, 2005, Shinohara et al.
J. Heinrich, et al., “Microstructure and Mechanical Properties of Reaction Bonded Silicon Nitride”, Energy and Ceramics, Proceedings of the 4thInternational Meeting on Modern Ceramics Technologies, XP-008063178, 1980, pp. 780-792.
U.S. Appl. No. 11/415,138, filed May 2, 2006, Shinohara et al.
U.S. Appl. No. 10/892,200, filed Jul. 16, 2004, Miyakawa et al.
U.S. Appl. No. 10/216,815, filed Aug. 13, 2002, Miyakawa et al.
U.S. Appl. No. 09/975,262, filed Oct. 12, 2001, Miyakawa.
U.S. Appl. No. 10/140,162, filed May 8, 2002, Miyakawa.
U.S. Appl. No. 10/901,171, filed Jul. 29, 2004, Shinohara et al.
U.S. Appl. No. 10/900,090, filed Jul. 28, 2004, Matsuzaki et al.
U.S. Appl. No. 10/901,158, Jul. 29, 2004, Suzuki et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for producing a silicon nitride filter does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for producing a silicon nitride filter, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for producing a silicon nitride filter will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2813621

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.