ABSTRACT:
An aqueous solution of 1-30 weight % alkali metal silicate and 0.005-10 weight % nitrite is stable and well permeable into hardened cementitious material. When applying said aqueous solution on the surface of hardened cementitious structure having metallic armatures embedded therein, it is possible not only to form surface layer improved in compactness, strength, hardness, waterproofing and weathering for preventing deterioration thereof and repair deteriorated cementitious material but also to prevent said metallic armatures from rusting.
REFERENCES:
patent: 4443496 (1984-04-01), Obitsu et al.
Hori Takahiro
Obitsu Masamichi
Nissan Chemical Industries Ltd.
Page Thurman K.
LandOfFree
Method for preventing hardened cementitious material from deteri does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for preventing hardened cementitious material from deteri, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for preventing hardened cementitious material from deteri will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2174312