On the surface of a heat exchanging portion in a heat exchanger, a film made of a polyaniline is formed. When the heat exchanger operates, condensed water is adhered on the surface of the heat exchanger, and contacts the film made of the polyaniline. Accordingly, oxygen dissolved in the condensed water becomes active oxygen by the polyaniline, and organic substances contained in the condensed water is decomposed. Thus, an amount of organic substances attached to a surface of the heat exchanger can be reduced in low cost without equipment extension.
REFERENCES:
patent: 3336099 (1967-08-01), Czulak et al.
patent: 5070938 (1991-12-01), Mizuno et al.
patent: 5741887 (1998-04-01), Morita et al.
patent: 5904990 (1999-05-01), Stenger-Smith et al.
patent: 5922466 (1999-07-01), Angelopoulos et al.
patent: 5976419 (1999-11-01), Hawkins et al.
patent: A8-296992 (1996-11-01), None
patent: 9-175801 (1997-07-01), None
patent: 10-316403 (1998-12-01), None
Kobayashi Kengo
Kuno Hitoshi
Morita Ken-ichi
Nagasawa Toshiya
Okamoto Yasushi
Denso Corporation
Harness Dickey & Pierce PLC
Morita Ken-ichi
Walberg Teresa J.
LandOfFree
Method for preventing contamination of heat exchanger and... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for preventing contamination of heat exchanger and..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for preventing contamination of heat exchanger and... will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-3398961