Method for preparing mixed amorphous vanadium oxides and their u

Chemistry: electrical current producing apparatus – product – and – Current producing cell – elements – subcombinations and... – Electrode

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

H01M 448

Patent

active

057005982

ABSTRACT:
A method for preparing an amorphous ternary lithiated vanadium metal oxide of the formula Li.sub.x M.sub.y V.sub.z O.sub.(x+5z+ny)/2, where M is a metal, 0<x.ltoreq.3, 0<y.ltoreq.3, 1.ltoreq.z.ltoreq.4, and n=2 or 3, comprising the steps of creating an aqueous solution of at least one metavanadate salt selected from the group consisting of NH.sub.4 VO.sub.3 and NaVO.sub.3, and a nitrate salt of the formula M(NO.sub.3).sub.n containing a large excess of a lithium salt; heating the solution; adding a sufficient amount of a base to obtain a suitable pH; and precipitating the amorphous lithiated vanadium metal oxide. A rechargeable lithiated intercalation battery cell comprising a positive electrode, a negative electrode, and an electrolyte, wherein the active material of the negative electrode is an amorphous ternary lithiated vanadium metal oxide of the formula Li.sub.x M.sub.y V.sub.z O.sub.(x+5z+ny)/2 or an amorphous binary non-lithiated vanadium metal oxide of the formula M.sub.y V.sub.z O.sub.(5z+ny)/2, prepared according to the methods of the present invention.

REFERENCES:
patent: 4675260 (1987-06-01), Sakurai et al.
patent: 5039582 (1991-08-01), Pistoia
patent: 5284721 (1994-02-01), Beard
patent: 5334334 (1994-08-01), Koksbang
patent: 5453337 (1995-09-01), Willmann et al.
patent: 5498494 (1996-03-01), Takeuchi et al.
Chemical Abstracts Accession No. 105:899960 CA, Toboul et al. J. Therm. Anal. (1986), 31(1) 117-124 (month unknown), 1986.
Bhattacharya et al., Solid State Communications, vol. 91, No. 5 pp. 357-360, "Low Temperature Synthesis of a Bismuth Vanadium Oxide Isomorphous with B4V2011" (month unknown), 1994.
Prokupkova et al., J. Materials Science, 31 (1996) 3391-3395 (month unavailable), 1996.
Sigala et al., "Amorphous lithium metal vanadium oxide compounds . . . ", CA Accession No. 125:304946, FR 2725709, Apr. 19, 1996.
Sigala et al., "Synthesis and performances of new negative electrode materials . . . ", CA Accession No. 123:61226, Inst. Mater. Nantes, Nantes, 44072, Fr. C.R. Acad.Sci., Ser.II: Mec., Phys., Chim., Astron. (1995), 320 (10), 523-9(month unavailable), 1995.
Myazaki et al., CA Accession No. 112: 81039 "Secondary lithium batteries", JP 012654456, Oct. 1989.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for preparing mixed amorphous vanadium oxides and their u does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for preparing mixed amorphous vanadium oxides and their u, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for preparing mixed amorphous vanadium oxides and their u will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1801411

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.