Method for preparing a lubricating composition based on...

Solid anti-friction devices – materials therefor – lubricant or se – Lubricants or separants for moving solid surfaces and... – Organic compound containing silicon

Reexamination Certificate

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C508S201000, C508S204000, C508S206000, C508S211000, C508S213000, C106S038220

Reexamination Certificate

active

07439211

ABSTRACT:
The invention concerns a method for preparing a lubricating composition, characterised in that it comprises mixing two previously prepared oil-in-water emulsions (A) and (B): the prior emulsion (A) comprises: (a) at least a non-reactive linear polyorganosiloxane oil comprising per molecule at least 2% in number of organic substituents bound to the silicon atoms which are aryl, alkylarylene and/or arylenealkyl radicals; (b) at least a polyorganosiloxane resin bearing hydroxyl groups and comprising at least two different siloxyl units selected among those formula (R1)3SiO1/2(M), (R1)2SiO2/2(D), R1SiO3/2(T) and SiO4/2(Q), one at least of said units being a unit T or Q, R1representing an organic substituent; (c) at least a crosslinking agent soluble in the silicone phase comprising at least two functions capable of reacting with the polyorganosiloxane resin(s) (b); (d) a condensation catalyst capable of catalysing the reaction of the constituent (b) with the constituent (c); (e) a surfactant; and (f) water; the prior emulsion (B) comprises: (a′) at least a reactive linear polyorganosiloxane oil comprising at least two OH groups per molecule, and the constituents (b), (c), (d), (e) and (f) mentioned above: each of the prior emulsions (A) and (B) comprises: 5 to 95 parts by weight of constituent (a) or (a′); 0.5 to 50 parts of constituent (b); 0.1 to 20 parts of constituent (c); 0.05 to 10 parts of constituent (d); for 100 parts of the sum (a)+(b)+(c)+(d) or (a′)+(b)+(c)+(d); the amounts of surfactant and water being sufficient to obtain an oil-in-water emulsion; and the weight ratio emulsion (A)/emulsion (B) ranges between 1.5 and 4.

REFERENCES:
patent: 4554122 (1985-11-01), Allardice
patent: RE32318 (1986-12-01), Comper et al.
patent: 5431832 (1995-07-01), Crowe et al.
patent: 6491981 (2002-12-01), Guichard et al.
patent: 6696392 (2004-02-01), Naik et al.
patent: 6825153 (2004-11-01), Giraud et al.
patent: 6846780 (2005-01-01), Giraud et al.
patent: 6933263 (2005-08-01), Manka et al.
patent: 0 399 526 (1990-11-01), None
patent: 0 635 559 (1995-01-01), None
patent: 0 279 372 (1998-08-01), None
patent: 1 000 989 (2000-05-01), None

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for preparing a lubricating composition based on... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for preparing a lubricating composition based on..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for preparing a lubricating composition based on... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-4014172

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.