ABSTRACT:
A method for preparing high molecular weight polyethermide polymers in a dual solvent system is disclosed. The inventive method provides for polymerizing a diamine monomer and a dianhydride monomer in a solvent system comprised of at least two solvents, a first solvent is selected for its solubility characteristics such that the polyethermide polymer is highly soluble therein and a second solvent is selected for its relatively high boiling point characteristics such that when the second solvent and first solvent are mixed together, the boiling point of the dual solvent system is at least as high as the temperature at which polymerization of said monomers occurs. In one embodiment, a diamine monomer of 4,4'-sulfonyl dianiline (SDAN) is reacted with a dianhydride monomer of bisphenol A dianhydride (BPADA) in the presence of a catalyst and a chain stopper in a dual solvent system comprised of chloroform and ortho-dichlorobenzene. The resulting polyethermide has an intrinsic viscosity exceeding 0.76 dl/g in chloroform at 25.degree. C.

REFERENCES:
patent: 3847867 (1974-11-01), Heath
patent: 3933749 (1976-01-01), Williams, III
patent: 3983093 (1976-09-01), Williams, III
patent: 4221897 (1980-09-01), Takekoshi
patent: 4417044 (1983-11-01), Parekh
patent: 4550156 (1985-10-01), Gallagher
patent: 4565858 (1986-01-01), Klopfer
patent: 4612361 (1986-09-01), Peters
patent: 4650850 (1987-03-01), Howson
patent: 4757150 (1988-07-01), Guggenheim

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for preparing a high molecular weight polyethermide polym does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for preparing a high molecular weight polyethermide polym, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for preparing a high molecular weight polyethermide polym will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2206080

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.