Adhesive bonding and miscellaneous chemical manufacture – Methods – Surface bonding and/or assembly therefor
Patent
1989-07-31
1990-09-18
Ball, Michael W.
Adhesive bonding and miscellaneous chemical manufacture
Methods
Surface bonding and/or assembly therefor
156121, 152503, 152506, B29C 7322, B29C 7300
Patent
active
049575732
ABSTRACT:
A self-healing tire containing an inner tube is obtained by a method comprising coating either the surface of the tube or the inner surface of a tire casing with a tacky, non-flowing sealant material. Prior to insertion of the inner tube, the surface of the sealant or the opposing surface of the tube or casing or both are coated with a anti-tack material, such as a plasticizer for the sealant. The anti-tack material renders the sealant non-tacky for a period of time long enough for insertion and inflation of the tube. However, the anti-tack material allows the sealant surface to become tacky again thereby adhering the tube to the casing and providing for sealing of the tube when it is punctured.
REFERENCES:
patent: 4396053 (1983-08-01), Davis
patent: 4664168 (1987-05-01), Hong et al.
Ball Michael W.
Wilber Gregory J.
LandOfFree
Method for placing an inner tube into a tire lined with sealant does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for placing an inner tube into a tire lined with sealant, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for placing an inner tube into a tire lined with sealant will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1570249