ABSTRACT:
The .alpha.-stabilizing element, e.g. P, and the .gamma.-stabilizing element, e.g. Mn, do not segregate at an identical site of a casting. Castings are cooled at a rate of 40.degree. C./min or less in a temperature range of the peritectic reaction and/or the Ar.sub.4 transformation, thereby condensing P and Mn into .delta. and .gamma. phases, respectively.

REFERENCES:
patent: 3771584 (1973-11-01), Wojcik

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for mitigating solidification segregation of steel does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for mitigating solidification segregation of steel, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for mitigating solidification segregation of steel will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2170214

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.