ABSTRACT:
Using a strain gauge attached at an interior side of a cylinder bore at a siamese region, a plurality of output values of the strain gauge can be detected during partially cutting the cylinder bore and residual stress of the siamese region can be calculated based on the plurality of the output values.

REFERENCES:
patent: 11-304603 (1999-11-01), None
patent: 1019990051769 (1999-07-01), None

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for measuring residual stress in a siamese region of... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for measuring residual stress in a siamese region of..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for measuring residual stress in a siamese region of... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3581798

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.