ABSTRACT:
A method for manufacturing a low carbon ferrochrome with a high chromium content of at least 70 weight % Cr comprising the steps of at least once nitriding and crushing a low carbon ferrochrome to form a crushed ferrochrome nitride and subjecting the crushed ferrochrome nitride to an acid treatment comprising introducing the crushed ferrochrome nitride into an acid solution and stirring the resultant mixture of the ferrochrome nitride and the acid solution, to remove iron. The acid treated ferrochrome nitride is denitrided by heating in a vacuum.

REFERENCES:
patent: 3384455 (1968-05-01), Fuchs
patent: 3525608 (1970-08-01), Bryk
patent: 4417927 (1983-11-01), Fullman

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for manufacturing low carbon ferrochrome with high chromi does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for manufacturing low carbon ferrochrome with high chromi, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for manufacturing low carbon ferrochrome with high chromi will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-930488

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.