ABSTRACT:
A method for manufacturing an anisotropic conductive adhesive sheet is disclosed. The sheet comprises at least a curing agent, a curable insulating resin, and conductive particles. The method comprises providing an adhesive layer on a biaxially stretchable film to form a laminate, densely packing conductive particles having an average particle size of 1 to 8 μm on the laminate to form a conductive particle-attached film, biaxially stretching and holding the conductive particle-attached film so that the average particle distance between adjacent conductive particles is at least one to five times or less the average particle size of the conductive particles and not greater than 20 μm. The conductive particles are transferred to an adhesive sheet containing at least a curing agent and a curable insulating resin and having a thickness of at least 1.5 times the average particle distance between the conductive particles but not greater than 40 μm.
REFERENCES:
patent: 5240761 (1993-08-01), Calhoun et al.
patent: 5362421 (1994-11-01), Kropp et al.
patent: 6020059 (2000-02-01), Yamada et al.
patent: 7416822 (2008-08-01), Kanada et al.
patent: 7625969 (2009-12-01), Sonobe et al.
patent: 7671142 (2010-03-01), Maekawa
patent: 2001/0008169 (2001-07-01), Connell et al.
patent: 2007/0029256 (2007-02-01), Nakano et al.
patent: 2007/0093583 (2007-04-01), Kakegawa
patent: 2007/0129484 (2007-06-01), Horio et al.
patent: 2007/0175579 (2007-08-01), Otani et al.
patent: 1128040 (1996-07-01), None
patent: 1307625 (2001-08-01), None
patent: 2-117980 (1990-05-01), None
patent: 6-045024 (1994-02-01), None
patent: 6-060712 (1994-03-01), None
patent: 6-349339 (1994-12-01), None
patent: 2895872 (1999-03-01), None
patent: 11-121072 (1999-04-01), None
patent: 2000-149677 (2000-05-01), None
patent: 2000-178511 (2000-06-01), None
patent: 3165477 (2001-03-01), None
patent: 2002-519473 (2002-07-01), None
patent: 2002-358825 (2002-12-01), None
patent: 2003-064324 (2003-03-01), None
International Search Report for PCT/JP2004/017944, mailed Feb. 15, 2005.
Chinese Office Action issued with respect to patent family member Chinese Application No. 200910117908.X, issued Dec. 16, 2010, along with an English-language translation.
Japanese Office Action issued with respect to Japanese Patent Application No. 2005-515962, issued Mar. 23, 2011.
Matsuura Koya
Otani Akira
Asahi Kasei EMD Corporation
Greenblum & Bernstein PLC
Parker Frederick
LandOfFree
Method for manufacturing an anisotropic conductive adhesive... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for manufacturing an anisotropic conductive adhesive..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for manufacturing an anisotropic conductive adhesive... will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-4293524