ABSTRACT:

FIELD OF THE INVENTION
The present invention relates to a method for manufacturing a semiconductor device which includes a non-single crystalline semiconductor layer formed on a substrate, for example, an insulating substrate such as glass. In particular, the semiconductor device is of an insulated gate type such as a thin film transistor (TFT) or thin film diode (TFD). The present invention is further related to a manufacture of a thin film integrated circuit utilizing the TFT or TFD, specifically a thin film integrated circuit for an active matrix liquid crystal display device.
DESCRIPTION OF PRIOR ART
In recent years, active matrix liquid crystal device and an image sensor have been developed which utilize a semiconductor device having TFTs formed on an insulating substrate such as glass for driving pixels or as a peripheral circuit.
Silicon in the form of a thin film is most generally used for forming TFTs of these semiconductor devices. Generally, thin film silicon semiconductors are classified to (a) amorphous silicon and (b) crystalline silicon. While amorphous silicon is easy to form at a relatively low temperature, electrical characteristics of the amorphous silicon is inferior to crystalline silicon.
In usual, when manufacturing TFTs with a silicon film, a pattering of the silicon film has been used to isolate each element from one another. A photoresist has been used to pattern the silicon film as a mask.
On the other hand, it has been strongly required to avoid any contamination of silicon during the fabrication process of TFTs as much as possible since an active semiconductor region of a TFT is very sensitive to impurities. As a source of a contamination, the air and the handling with human hands are known. However, this problem has not been completely solved yet.
SUMMARY OF THE INVENTION
It is an object of the present invention to provide a semiconductor device such as a TFT or image sensor having a high quality by solving the foregoing problems.
It is another object of the present invention to provide a semiconductor device having a semiconductor film with an improved crystallinity.
The inventors of the present invention first recognized that a photoresist which is used for patterning a semiconductor layer is one of the sources of the contamination causing properties of the TFTs degrade. Based on this recognition, the primary feature of the invention is to provide a protective film between the photoresist and the semiconductor layer in order to prevent the impurity elements contained in the photoresist from invading into the semiconductor layer.


REFERENCES:
patent: 4059461 (1977-11-01), Fan et al.
patent: 4132571 (1979-01-01), Cuomo et al.
patent: 4151008 (1979-04-01), Kirkpatrick
patent: 4174217 (1979-11-01), Flatley
patent: 4271422 (1981-06-01), Ipri
patent: 4277884 (1981-07-01), Hsu
patent: 4292091 (1981-09-01), Togei
patent: 4534820 (1985-08-01), Mori et al.
patent: 4544418 (1985-10-01), Gibbons
patent: 4755481 (1988-07-01), Faraone
patent: 5004701 (1991-04-01), Motokawa
patent: 5147826 (1992-09-01), Liu et al.
patent: 5173446 (1992-12-01), Asakawa et al.
patent: 5275851 (1994-01-01), Fonash et al.
patent: 5403772 (1995-04-01), Zhang et al.
patent: 5508533 (1996-04-01), Takemura
patent: 5550070 (1996-08-01), Funai et al.
patent: 5637515 (1997-06-01), Takemura
patent: 5888857 (1999-03-01), Zhang et al.
patent: 5985704 (1999-11-01), Adachi et al.
patent: 6171890 (2001-01-01), Adachi et al.
patent: 57-028357 (1982-02-01), None
patent: 62-042535 (1987-02-01), None
patent: 63-142807 (1988-06-01), None
patent: 1-187874 (1989-07-01), None
patent: 1-187875 (1989-07-01), None
patent: 2-140915 (1990-05-01), None
patent: 2-275641 (1990-11-01), None
patent: 3-280418 (1991-12-01), None
patent: 3-292741 (1991-12-01), None
patent: 5-291295 (1993-11-01), None
Wolf et al., Silicon Processing for the VLSI Era vol. 1: Process Technology, Lattice Press, Sunset Beach, CA, USA, pp. 198-219, 303-307, 407-409, 1986.*
S. Lau et al., “Solid Phase Epitaxy In Silicide-Forming Systems”,Thin Sold Films, 47 (1977), pp. 313-322.
Y. Kawazu et al., “Low Temperature Crystallization of Hydrogenated Amorphous Silicon Induced by Nickel Silicide Formation”, Japanese Journal of Applied Physics, vol. 29, No. 12, Dec. 1990, pp. 2698-2704.
I.W. Boyd et al., “Oxidation of silicon surfaces by CO2lasers”, Applied Physics Letters, vol. 41, No. 2, Jul. 15, 1982, pp. 162-164.
S. Wolf et al., “Silicon Processing for the VLSI Era”, Lattice Press, 1986, vol. 1, pp. 198-219, 303-307.
S.K. Ghandhi, “VLSI Fabrication Principles”, John Wiley & Sons, 1983, pp. 419-429
P. Zorabedian et al., “Lateral Seeding of Silicon-on-Insulator using an Elliptical Laser Beam: a Comparison of Scanning Methods”, Mat. Res. Soc. Symp. Proc. vol. 33, 1984, Lam et al. Ed, pp. 81-86.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for manufacturing a semiconductor device does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for manufacturing a semiconductor device, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for manufacturing a semiconductor device will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3087666

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.