Method for making solid materials having a flash point of less t

Stock material or miscellaneous articles – Web or sheet containing structurally defined element or... – Composite having voids in a component

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

521 59, 521 57, 521 54, 521 55, 264 451, 264 453, 264 459, 428407, 252 8, 252408, 116 23, 116101, C08G 800

Patent

active

042308089

ABSTRACT:
Solid materials having a flash point of less than 500.degree. C. are rendered fire alarming by providing for the presence thereon of micro capsules containing a bromofluoroalkane having a critical temperature of at least 100.degree. C., the micro capsules having an external diameter of from 200 to 260 microns, and the wall of the capsules consisting of a polymer, treated to release the bromofluoralkane suddenly at a predetermined temperature to provide a detonation having a maximum sound level of 10-12 kHz.

REFERENCES:
patent: 4024092 (1977-05-01), Sonnenberg
patent: 4026829 (1977-05-01), Samura et al.
patent: 4035315 (1977-07-01), Ingram
patent: 4122203 (1978-10-01), Stahl

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for making solid materials having a flash point of less t does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for making solid materials having a flash point of less t, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for making solid materials having a flash point of less t will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-268860

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.