Method for making sintered dolomite with a low porosity and a go

Compositions: ceramic – Ceramic compositions – Refractory

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

501113, 501123, 501125, C04B 3504

Patent

active

043944540

ABSTRACT:
To produce a dolomite sinter with a low porosity and a good hydration stability made of difficult-to-sinter raw dolomite, the dolomite is milled and caustic burnt dolomite, dolomite hydrate or semi-burnt dolomite in quantities between 3 and 20% by weight relative to the total mixture is added to the raw dolomite powder and is calculated as oxide, as well as foreign oxide, such as Fe.sub.2 O.sub.3, Al.sub.2 O.sub.3 or SiO.sub.2, in such quantities that the total content of the foreign oxide mixture is 1 to 3% by weight.

REFERENCES:
patent: 2133672 (1938-10-01), Singewald

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for making sintered dolomite with a low porosity and a go does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for making sintered dolomite with a low porosity and a go, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for making sintered dolomite with a low porosity and a go will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-752092

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.