ABSTRACT:
A method for making a cast iron product having a high resistance to both wear and pitting. The method comprises casting a cast iron containing C, Si, Mn, Cu, Ni, Cr and Mo with or without P and S to provide a casting having a local chilled structure having a cementite content of 30 to 50%. The casting is then annealed at a reduced temperature and subsequently subjected to a quenching treatment. The quenching treatment is carried out by heating the casting under a particular condition including heating temperature and time and then quenching it. The product is finally tempered.
REFERENCES:
patent: 2962397 (1960-11-01), Thompson
patent: 4032334 (1977-06-01), Burk et al.
patent: 4124413 (1978-11-01), Komatsu et al.
Marbaker E., "Heat Treatment of Gray Cast Iron", Iron Age, Aug. 2, 1928.
Yamamoto Yukio
Yoritaka Masashi
Brody Christopher W.
Mazda Motor Corporation
Rutledge L. Dewayne
LandOfFree
Method for making pitting resistant cast iron product does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for making pitting resistant cast iron product, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for making pitting resistant cast iron product will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2359282