ABSTRACT:
BACKGROUND OF THE INVENTION
Thin film inductive heads are used to read and write data to and from an adjacent disc surface. Typically, the inductive head includes a top and bottom magnetic pole separated by a gap of insulating material, with a conductive coil embedded in the insulating material of the gap distal from the air bearing surface (ABS) of the head. Typically, the bottom pole and insulating gap are not of critical dimension to the width of the recording track, as the track width is defined by the width of the top magnetic pole at the air bearing surface. (Of course, the thickness of the insulating material forming the gap is critical since it defines the bit length of the recorded track.)
The elements of the thin film inductive head are usually formed by a photolithographic process. The photolithographic mask defining the top pole piece includes a trench that extends from the paddle region of the pole (where the coils form a hill in the insulating material) to the ABS. The trench defines the width of the top pole piece at the ABS, and hence the width of the track. As track width dimensions become smaller and the radial track density (number of tracks per inch) increases, the aspect ratio of the trench pattern in the photoresist forming the top pole piece becomes increasingly critical. More particularly, the top pole is created by depositing the magnetic material into the trench in the photolithographic mask formed on the insulating layer. If the trench is not well defined, or if it includes debris, the resulting top pole piece is not well defined at the ABS, leading to adverse operation of the head. Typically, the photolithographic mask is quite thick (about 13 microns) compared to the width of the mask trench at the gap (typically less than about 2 microns).
The photolithographic mask is ordinarily formed by spinning the photolithographic material, such as a photoresist, onto the insulating layer of the head to a thickness of about 13 microns. The coil configuration within the head forms a sloped hill portion to the insulating layer having a raised portion (where the paddle region of the top pole will be placed) and sloping downhill to the gap at the ABS. In forming the mask, the photoresist is spun over the hill, including on the slope, and past the intended ABS to a waste area. The photolithographic material is then patterned to the shape of the desired pole over the insulating material, to define the paddle and gap regions of the pole and a feeder region in the waste area. The photolithographic material is then exposed and thereafter washed out with a solvent. Typically, the solvent is applied to the exposed portions of the photoresist at the paddle region and in the feeder region and allowed to flow from the feeder region, through the trench area and into the paddle region. However, the flow of the solvent through the trench region of the photoresist often creates residue in that trench region, resulting in a poorly defined trench and adversely affecting the deposit of magnetic material within the trench to define the gap at the air bearing surface. As a result, when the head is later diced and milled at the ABS, unwanted residue within the mask inhibits proper formation of the magnetic pole at the gap, resulting in unacceptable performance of the head.
To achieve a well-defined, acceptably clear trench for formation of the gap region of the top pole piece, the solvent must be evenly applied to the photolithographic mask material. This requirement has heretofore been a limiting factor on the width of the trench, and hence the width of the top pole piece at the ABS. For this reason, it is not been practical, prior to the present invention, to achieve gap widths for inductive magnetic heads less than about 1.8 microns. We have discovered, however, that trenches with smaller widths and higher aspect ratios (height to width) can be achieved by applying a laminar flow of the solvent through the trench.
BRIEF SUMMARY OF THE INVENTION
In accordance with one form of the invention, a mask forms a top magnetic pole piece of an inductive magnetic head on a wafer. The magnetic head has a layer of insulating material over a hill region and a gap region, and the mask comprises a layer of photolithographic material on the insulating material and a waste region of the wafer. The mask comprises an aperture exposing the insulating material to define a paddle region of the pole piece over the hill region and a trench over the gap region. Means connected to the aperture defines a feeder region over the waste region that provides laminar flow of solvent from the feeder region to and through the trench.
In one embodiment of this form of the invention, the means defining the feeder region comprises a second aperture having walls for funneling solvent in a non-turbulent flow into and through the feeder region.
In another form of the invention, the top magnetic pole of an inductive magnetic head is formed on a wafer by forming a photolithographic material on the wafer that extends over the layer of insulating material at the hill region and gap region of the inductive magnetic head and over the waste region of the wafer. A mask is patterned on the photolithographic material to define a paddle region over the hill region, a feeder region over the waste region, and a trench region extending over the gap region between the feeder region and the paddle region. Solvent is admitted into the feeder region to flow in a laminar flow through the trench region to the paddle region to form the mask and expose a surface of the layer of insulating material in the paddle and trench regions of the mask.
In a preferred embodiment of this form of the invention, the feeder region includes walls tapered to funnel solvent into the trench region in a non-turbulent flow. Optimally, the trench region has an average width not greater than 1.0 microns. In one form of the invention magnetic material is deposited on the exposed surface of the layer of insulating material, and the waste region of the wafer, including magnetic material deposited on the waste region, may be removed to define an air bearing surface of the head at the gap region.
In another form of the invention, the mask and process from a top pole piece of an inductive magnetic head, wherein the top pole piece defines a gap width at an air bearing surface having an average track width not greater than 1.0 microns. Optimally, the standard deviation of the average gap widths of magnetic heads is no more than 0.07 for heads formed on a single wafer and no more than 0.12 for heads formed on different wafers.
REFERENCES:
patent: 4418472 (1983-12-01), Lorenze, Jr.
patent: 5245493 (1993-09-01), Kawabe et al.
patent: 5446613 (1995-08-01), Rottmayer
patent: 5452164 (1995-09-01), Cole et al.
patent: 5559654 (1996-09-01), Das
patent: 5600880 (1997-02-01), Santini et al.
patent: 5614438 (1997-03-01), Evans, Jr. et al.
patent: 5649351 (1997-07-01), Cole et al.
patent: 5719730 (1998-02-01), Chang et al.
patent: 5752309 (1998-05-01), Partee et al.
patent: 5763108 (1998-06-01), Chang et al.
patent: 5804085 (1998-09-01), Wu et al.
patent: 5820770 (1998-10-01), Cohen et al.
patent: 5827775 (1998-10-01), Miles et al.
patent: 5831801 (1998-11-01), Shouji et al.
patent: 5843521 (1998-12-01), Ju et al.
patent: 5854727 (1998-12-01), Tanaka et al.
patent: 5867890 (1999-02-01), Hsiao et al.
patent: 5898540 (1999-04-01), Maruyama et al.
patent: 5932100 (1999-08-01), Yager et al.
patent: 5961832 (1999-10-01), Shaw et al.
patent: 5961848 (1999-10-01), Jacquet et al.
patent: 6016242 (2000-01-01), Mastain et al.
patent: 6120942 (2000-09-01), Reinberg
patent: 6129855 (2000-10-01), Sawada et al.
patent: 6287475 (2001-09-01), Fukushima et al.
Mastain Steven A.
Peck Wallace A.
Rothstein Kurt A.
Simplair Diana M.
Kinney & Lange , P.A.
Trinh Minh
LandOfFree
Method for making narrow top poles for inductive magnetic heads does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for making narrow top poles for inductive magnetic heads, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for making narrow top poles for inductive magnetic heads will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2884473