ABSTRACT:
The method produces low-stress, large-volume crystals with low birefringence and uniform index of refraction. The method includes growing the crystal with larger than desired dimensions including diameter and height from a melt; cooling and tempering the crystal with the larger than desired dimensions and after the cooling and tempering removing edge regions of the crystal with the larger than desired dimensions so that a diameter reduction and a height reduction of at least five percent occurs respectively and so that the crystal has the desired dimensions of diameter and height. No further tempering takes place after removing of the edge regions.

REFERENCES:
patent: 6332922 (2001-12-01), Sakuma et al.
patent: 6364946 (2002-04-01), Staeblein et al.
patent: 6624390 (2003-09-01), Motakef et al.
patent: 6969502 (2005-11-01), Wehrhan et al.
patent: 7534412 (2009-05-01), Ortmann et al.
patent: 2002/0020338 (2002-02-01), Oba et al.
patent: 2002/0038625 (2002-04-01), Sakuma et al.
patent: 2002/0182863 (2002-12-01), Chiba
patent: 2003/0089307 (2003-05-01), Wehrhan et al.
patent: 2004/0005266 (2004-01-01), Sakuma et al.
patent: 2004/0016743 (2004-01-01), Motakef et al.
patent: 2004/0099205 (2004-05-01), Li et al.
patent: 2004/0154527 (2004-08-01), Li et al.
patent: 2005/0183659 (2005-08-01), Staeblein et al.
patent: 2005/0211160 (2005-09-01), Ortmann et al.
patent: 2007/0251443 (2007-11-01), Parthier et al.
patent: 213 514 (1984-09-01), None
patent: 100 10 484 (2001-09-01), None
patent: 100 10 485 (2001-09-01), None
patent: 10 2004 003 831 (2004-07-01), None
patent: 0 939 147 (1999-09-01), None
patent: 0 942 297 (1999-09-01), None
patent: 0 972 863 (2000-01-01), None
patent: 0 995 820 (2000-04-01), None
patent: 1 234 898 (2002-08-01), None
patent: 10251096 (1998-09-01), None
patent: 2001335398 (2001-12-01), None
patent: 2003-327499 (2003-11-01), None
Technical Information Advanced Optics, TIE-26: Homogenety of Optical Glass, Jul. 2004 (In English).
Metrology: Homogenety of Refractive Index; Stress Birefringence Retardation, Mar. 25, 2010 (In English).

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for making low-stress large-volume crystals with... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for making low-stress large-volume crystals with..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for making low-stress large-volume crystals with... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2664327

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.