ABSTRACT:
Discontinuous diamond particulate containing metal matrix composites of high thermal conductivity and methods for producing these composites are provided. The manufacturing method includes producing a thin reaction formed and diffusion bonded functionally graded interactive SiC surface layer on diamond particles. The interactive surface converted SiC coated diamond particles are then disposed into a mold and between the particles and permitted to rapidly solidify under pressure. The surface conversion interactive SiC coating on the diamond particles achieves minimal interface thermal resistance with the metal matrix which translates into good mechanical strength and stiffness of the composites and facilitates near theoretical thermal conductivity levels to be attained in the composite. Secondary working of the diamond metal composite can be performed for producing thin sheet product.

REFERENCES:
patent: 3520667 (1970-07-01), Taylor
patent: 3617347 (1971-11-01), Kuratomi
patent: 4606738 (1986-08-01), Hayden
patent: 4643741 (1987-02-01), Yu et al.
patent: 4783368 (1988-11-01), Yamamoto et al.
patent: 4914551 (1990-04-01), Anschel et al.
patent: 5676918 (1997-10-01), Okada et al.
patent: 5735332 (1998-04-01), Ritland et al.
patent: 5783316 (1998-07-01), Colella et al.
patent: 5855967 (1999-01-01), Kirkpatrick
patent: 6031285 (2000-02-01), Nishibayashi
patent: 6106957 (2000-08-01), Fang
patent: 6171691 (2001-01-01), Nishibayashi
patent: 6270848 (2001-08-01), Nishibayashi
patent: 6447852 (2002-09-01), Gordeev et al.
patent: 6673439 (2004-01-01), Miyamoto et al.
patent: 6727117 (2004-04-01), McCoy
patent: 6821495 (2004-11-01), Fukuoka et al.
patent: 6984888 (2006-01-01), Sung
patent: 2001/0015271 (2001-08-01), Lo et al.
patent: 2004/0053039 (2004-03-01), Ekstrom et al.
patent: 0 364 155 (1989-10-01), None
patent: 0 459 474 (1991-05-01), None
patent: 1 143 044 (2001-10-01), None
patent: 4-19072 (1992-01-01), None
patent: 8-113774 (1996-05-01), None
patent: H10-223812 (1998-08-01), None
patent: 2003-095743 (2003-04-01), None
patent: WO 01/21862 (2001-03-01), None
European Supplementary Search Report, Appln. No. 04809792.7, dated Dec. 29, 2010 (3 pages).
Official Action translation dated Nov. 22, 2010, issued in corresponding Japanese application No. 2006- 533975 (1 pg).
Office Action of U.S. Appl. No. 12/688,454 dated Dec. 29, 2010 (15 pages).
Official Action dated Apr. 29, 2011, U.S. Appl. No. 12/688,454.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for making high thermal conductivity metal matrix... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for making high thermal conductivity metal matrix..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for making high thermal conductivity metal matrix... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-4295779

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.