ABSTRACT:
A fine grained alloy containing 38-45% nickel, 3-15% chromium, up to 0.1% copper, from 0.1-1.0% titanium and the balance iron and residuals that is useful for production of glass-to-metal seals is disclosed.

REFERENCES:
patent: 1489243 (1924-04-01), Giring
patent: 2266482 (1941-12-01), Pilling
patent: 2730260 (1956-01-01), McCullough
patent: 2793948 (1957-05-01), Wagner
patent: 3366473 (1960-01-01), Nehrenberg
patent: 3843332 (1974-10-01), Kindlimann

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for making fine grained metals for glass-to-metal seals does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for making fine grained metals for glass-to-metal seals, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for making fine grained metals for glass-to-metal seals will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1574537

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.