Method for making cylindrical, iron-based sintered slugs of spec

Metal treatment – Process of modifying or maintaining internal physical... – Treating consolidated metal powder – per se

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

148902, 419 41, 419 67, B22F 900, C22F 100

Patent

active

052019667

ABSTRACT:
A cylindrical, iron-based sintered slug comprising an iron-based sintered alloy having a surface hardness represented by an HRB of 40-90 is formed such that its interior porosity is 5% or less but greater than 0%, the porosities of both its surface layer regions lying at most 1 mm below its outer and inner surfaces are fixed at at least 3% or less but greater than 0% and the distribution of pores in each of the surface layers is decreased gradually toward the surface.

REFERENCES:
patent: 3901661 (1975-08-01), Kondo et al.
patent: 4018632 (1977-04-01), Schmidt
patent: 4364162 (1982-12-01), Nilsson et al.
patent: 4867807 (1989-09-01), Torisaka et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for making cylindrical, iron-based sintered slugs of spec does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for making cylindrical, iron-based sintered slugs of spec, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for making cylindrical, iron-based sintered slugs of spec will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1152859

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.