ABSTRACT:
This invention relates to a method where sulfidic iron-bearing copper concentrate is leached on the countercurrent principle, in a chloride environment. The leaching takes place with the aid of bivalent copper and an oxygen-bearing gas as a multi-stage continuous process, under normal pressure, at a temperature, which as highest corresponds to the boiling point of the solution. Part of the insoluble solid matter is returned, counter to the main flow of solid matter, to one of the previous leaching stages or reactors where, as a result of the extended leaching time, the leach waste iron is recovered mostly as hematite.

REFERENCES:
patent: 3972711 (1976-08-01), Goens et al.
patent: 4148698 (1979-04-01), Everett
patent: 4197117 (1980-04-01), Pemsler et al.
patent: 5487819 (1996-01-01), Everett
patent: 6007600 (1999-12-01), Hyvarinen et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for leaching copper concentrate does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for leaching copper concentrate, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for leaching copper concentrate will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3508077

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.