ABSTRACT:
Method and apparatus for inhibiting stress corrosion cracking adjacent weldments in steel workpieces such as stainless steel pipe through generation of a controllable throughwall temperature differential by exposure of one workpiece surface to externally generated radiant heat while maintaining a flow of coolant fluid past the other surface thereof.

REFERENCES:
patent: 3567907 (1971-03-01), Carpenter
patent: 4188419 (1980-02-01), Deteit et al.
patent: 4229235 (1981-10-01), Matsuda et al.
patent: 4354883 (1987-10-01), Terasaki

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for inhibiting stress corrosion cracking does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for inhibiting stress corrosion cracking, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for inhibiting stress corrosion cracking will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-460368

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.