Method for improving the hemmability of age-hardenable aluminum

Metal treatment – Process of modifying or maintaining internal physical... – Heating or cooling of solid metal

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

148691, 148694, 148688, 148695, 148417, 148415, 148416, C22C 2100

Patent

active

059481854

ABSTRACT:
An improved method of forming a severe bend or a hem in a sheet of wrought aluminum age-hardened and age-hardenable alloy includes heating the region to be bent or hemmed to a temperature above about 250.degree. C. for a period of seconds and then quenching the heated region to remove the age-hardening effect and thereafter accomplishing the bend or hem before age hardening of the heated region occurs.

REFERENCES:
patent: 3856584 (1974-12-01), Cina
patent: 3945861 (1976-03-01), Anderson et al.
patent: 4405386 (1983-09-01), Mravic et al.
patent: 4766664 (1988-08-01), Benedyk
patent: 5525169 (1996-06-01), Murtha
Element of materials science Van Vlack. pp. 275-313, .COPYRGT.1964.
ASM Metals Handbook 9th ed. vol. 2 pp. 24-32 & 50-51.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for improving the hemmability of age-hardenable aluminum does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for improving the hemmability of age-hardenable aluminum , we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for improving the hemmability of age-hardenable aluminum will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1800852

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.