ABSTRACT:
The density and crush resistance of calcined coke are improved by depositing coker feedstock on green (uncalcined) coke, thereafter subjecting the coke to a heat soak and then calcining the coke.

REFERENCES:
patent: 2582764 (1952-01-01), Bailey
patent: 3257309 (1966-06-01), Fauchier et al.
patent: 3401089 (1968-09-01), Friedrich et al.
patent: 3759795 (1973-09-01), Oliver et al.
patent: 3957957 (1976-05-01), Newman et al.
patent: 3996108 (1976-12-01), Joseph
patent: 4148692 (1979-04-01), Chu et al.
patent: 4202734 (1980-05-01), Greenbaum
patent: 4521278 (1985-06-01), Kelley et al.
patent: 4545859 (1985-10-01), Kelley et al.
patent: 4547284 (1985-10-01), Sze et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for improving the density and crush resistance of coke does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for improving the density and crush resistance of coke, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for improving the density and crush resistance of coke will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1038323

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.