ABSTRACT:
A method for producing an annealing separator coating on grain oriented silicon steel prior to final texture annealing to improve the coating uniformity and prevent oxidation of the steel surface during this annealing operation. The method comprises coating the steel with a conventional coating, such as magnesium oxide, having an addition of an inert, high temperature refractory annealing separator agent, preferably calcined alumina.
An annealing separator composition is also provided.
REFERENCES:
patent: 3379581 (1968-04-01), Kohler et al.
patent: 3544396 (1970-12-01), Taylor
patent: 3615918 (1971-10-01), Evans
patent: 3956029 (1976-05-01), Yamamoto et al.
patent: 4010050 (1977-03-01), Choby
patent: 4113530 (1978-09-01), Shimanaka et al.
patent: 4179315 (1979-12-01), Miller
patent: 4200477 (1980-04-01), Datta et al.
patent: 4255205 (1981-03-01), Morito et al.
patent: 4287006 (1981-09-01), Hiromae et al.
patent: 4344802 (1982-08-01), Haselkorn
patent: 4443425 (1984-04-01), Sopp et al.
Allegheny Ludlum Steel Corporation
Sheehan John P.
Viccaro Patrick J.
LandOfFree
Method for improving the annealing separator coating on silicon does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for improving the annealing separator coating on silicon , we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for improving the annealing separator coating on silicon will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1437022