ABSTRACT:
This invention is directed toward a method for improving the green strength properties of vulcanizable rubber compositions comprising the step of mixing a halogenated polymer with the vulcanizable rubber composition prior to curing in an amount ranging from about 5 to 25 weight percent of the rubber in the composition.
REFERENCES:
patent: 2729608 (1956-01-01), Strain
patent: 3714296 (1973-01-01), Kitagowa et al.
patent: 3827991 (1974-08-01), Ando et al.
patent: 3943193 (1976-03-01), Miyagawa et al.
patent: 4048261 (1977-09-01), Starmer
patent: 4254013 (1981-03-01), Friedman et al.
patent: 4267079 (1981-05-01), Davis et al.
patent: 4309332 (1982-01-01), Fischerelal
patent: 4316825 (1982-02-01), Wirth
patent: 4421900 (1983-12-01), Hamed
patent: 4454204 (1984-06-01), Tsai
patent: 4584350 (1986-04-01), Davis
Hall Daniel N.
Lieberman Allan M.
The Firestone Tire & Rubber & Company
LandOfFree
Method for improving green strength properties of vulcanizable r does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for improving green strength properties of vulcanizable r, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for improving green strength properties of vulcanizable r will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1278403