ABSTRACT:
Reduction of yellowing and improvement of impact strength are obtained during the processing of nitrile polymers when said polymers are heated to a plastic state in the presence of an inert gas, thereby excluding oxygen.
REFERENCES:
patent: 2445042 (1948-07-01), Silverman
patent: 3426102 (1969-02-01), Solak et al.
patent: 3586737 (1971-06-01), Duke et al.
patent: 3763278 (1973-10-01), Griffith
Bond Thomas J.
Feldman Daniel W.
Talsma Herbert
Evans Larry W.
Knudsen Herbert D.
Levin Stanford M.
Standand Oil Company
Untener David J.
LandOfFree
Method for improving color and impact strength of nitrile polyme does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for improving color and impact strength of nitrile polyme, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for improving color and impact strength of nitrile polyme will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-716531