Method for filling metal into fine space

Metal working – Method of mechanical manufacture – Combined manufacture including applying or shaping of fluent...

Reexamination Certificate

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C029S527100, C029S527200, C029S527300, C029S527700, C029S530000, C164S007100, C164S034000, C164S061000, C164S113000, C228S221000, C228S227000, C228S245000, C228S246000

Reexamination Certificate

active

08079131

ABSTRACT:
The present invention includes a step of cooling a molten metal within a fine space present in the inside of an object and hardening it while applying a forced external force exceeding atmospheric pressure to the molten metal. The fine space is opened on the outer surface of the object in terms of one end thereof. The forced external force is given by at least one member selected among a pressing pressure, an injection pressure and a rolling compaction and applied to the molten metal from the opening surface side on which the fine space is opened, in a state that the other end side of the fine space is closed.

REFERENCES:
patent: 5908065 (1999-06-01), Chadwick
patent: 6178093 (2001-01-01), Bhatt et al.
patent: 6516862 (2003-02-01), Klein
patent: 6620264 (2003-09-01), Kundig et al.
patent: 6764748 (2004-07-01), Farquhar et al.
patent: 7217890 (2007-05-01), Suemasu et al.
patent: 7814651 (2010-10-01), Suemasu et al.
patent: 2005/0147522 (2005-07-01), Watanabe et al.
patent: 2-213471 (1990-08-01), None
patent: 3-225829 (1991-10-01), None
patent: 07-142283 (1995-06-01), None
patent: 11-298138 (1999-10-01), None
patent: 2000-111896 (2000-04-01), None
patent: 2000-228410 (2000-08-01), None
patent: 2001-053218 (2001-02-01), None
patent: 2002-158191 (2002-05-01), None
patent: 2002-237468 (2002-08-01), None
patent: 2002-368082 (2002-12-01), None
patent: 2002368082 (2002-12-01), None
patent: 2003-168859 (2003-06-01), None
patent: 2003-257891 (2003-09-01), None
patent: 2003-273155 (2003-09-01), None
patent: 2004-128042 (2004-04-01), None
patent: 2004-241479 (2004-08-01), None
patent: 2005-059061 (2005-03-01), None
patent: 2005-064451 (2005-03-01), None
patent: 2005-109515 (2005-04-01), None
patent: 2005-116863 (2005-04-01), None
patent: 2005-123240 (2005-05-01), None
patent: 2005-123250 (2005-05-01), None
patent: 2005-183548 (2005-07-01), None
patent: 2006-032695 (2006-02-01), None
patent: 2006-179711 (2006-07-01), None
patent: 2006-203170 (2006-08-01), None
patent: 2007-096226 (2007-04-01), None
patent: 2007-096232 (2007-04-01), None
patent: 2007-250867 (2007-09-01), None
patent: 2008-053429 (2008-06-01), None
Office Action issued Dec. 27, 2010, in Taiwan Patent Application No. 098116527 (with English translation).

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for filling metal into fine space does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for filling metal into fine space, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for filling metal into fine space will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-4314898

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.