ABSTRACT:
A metallic article made of metallic constituent elements is fabricated from a mixture of nonmetallic precursor compounds of the metallic constituent elements. The mixture of nonmetallic precursor compounds contains more of a base-metal element, such as nickel, cobalt, iron, iron-nickel, and iron-nickel-cobalt than any other metallic element. The mixture of nonmetallic precursor compounds is chemically reduced to produce a metallic superalloy material, without melting the metallic superalloy material. The metallic superalloy material is consolidated to produce a consolidated metallic article, without melting the metallic superalloy material and without melting the consolidated metallic article.
REFERENCES:
patent: 2937979 (1960-05-01), Wainer
patent: 4383852 (1983-05-01), Yoshizawa
patent: 4415528 (1983-11-01), Wiech, Jr.
patent: 4519839 (1985-05-01), Toyoaki et al.
patent: 4894086 (1990-01-01), Huether et al.
patent: 5322666 (1994-06-01), Watwe
patent: 5779761 (1998-07-01), Armstrong et al.
patent: 5930580 (1999-07-01), Everett
patent: 5958106 (1999-09-01), Armstrong et al.
patent: 6926754 (2005-08-01), Shamblen et al.
patent: 6926755 (2005-08-01), Shamblen et al.
patent: 6968990 (2005-11-01), Ott et al.
patent: WO99/64638 (1999-12-01), None
Doyle, Eoghan T.M. et al. “Carbothermic reduction of nickel-cobalt-chromium oxide mixture for the production of NiCoCr superalloy powder” EPD Congr. 1992, Proc. Symp. TMS Annu. Meet., 745-58. Editor(s): Hager, John P.; Publisher: Miner. Met. Mater. Soc., Warrendale, PA. Coden: 58HHA7, 1992, XP0009029023.
Gerdemann et al., Characterization of a Titanium Powder Produced Through a Novel Continuous Process, U.S. Department of Energy, Albany Research Center, Albany, Oregon, 2000, pp. 12-44 through 12-52, USA.
Moxson et al., Producton, Characterization and Application of Low Cost Titanium Powder Products, the Minerals, Metals & Materials Society, 1998, pp. 127-134, USA.
Baburaj et al., Production of Low Cost Titanium, The Minerals, Metals & Materials, 1998, pp. 89-97, USA.
Gerdemann, Steven J., Titanium Process Technologies, Advanced Materials & Processes, Jul. 2001, pp. 41-43, USA.
Gigliotti Michael Francis Xavier
Ott Eric Allen
Shamblen Clifford Earl
Woodfield Andrew Philip
King Roy
Mai Ngoclan T.
McNees Wallace & Nurick LLC
LandOfFree
Method for fabricating a superalloy article without any melting does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for fabricating a superalloy article without any melting, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for fabricating a superalloy article without any melting will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-3965213