Method for expelling entrapped air from reactive metallic layups

Metal fusion bonding – Process – With protecting of work or filler or applying flux

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

228157, 228193, B23K 3538, B23K 1900

Patent

active

045000336

ABSTRACT:
In a process for diffusion bonding of at least two metal workpieces of a reactive metal, particularly titanium, the improvement for expelling entrapped air from between surfaces of such workpieces prior to diffusion bonding, which comprises precoating the metal surfaces of the workpieces which are to be diffusion bonded with a substance capable of decomposing at a temperature above about 800.degree. F. and below the diffusion bonding temperature of the workpieces, e.g. of the order about 1300.degree. F., such substance being preferably polytetrafluoroethylene, to form an inert gas having a density greater than air, heating the workpieces to a temperature above about 800.degree. F. and causing decomposition or pyrolysis of such substance and forming an inert gas having a density greater than air, and flushing the inert gas together with the entrapped air out of contact with the surfaces of the workpieces, preferably by means of argon having a density greater than the pyrolysis products or the inert gas. The workpieces are further heated to cause diffusion bonding of the workpieces.

REFERENCES:
patent: 2561566 (1951-07-01), Edson et al.
patent: 3468016 (1969-09-01), Lorain et al.
patent: 3916506 (1975-11-01), Wolf
patent: 3927817 (1975-12-01), Hamilton et al.
patent: 3937387 (1976-02-01), Fletcher et al.
patent: 4324594 (1982-04-01), Chasteen

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for expelling entrapped air from reactive metallic layups does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for expelling entrapped air from reactive metallic layups, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for expelling entrapped air from reactive metallic layups will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-608771

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.