Coating processes – Pretreatment – per se – or post-treatment – per se
Patent
1996-05-29
1997-09-30
King, Roy V.
Coating processes
Pretreatment, per se, or post-treatment, per se
427249, 427577, 4273722, B05D 300
Patent
active
056723954
ABSTRACT:
A method for treating as as-grown chemical vapor deposited (CVD) starting diamond film having stresses and containing voids, comprises the step of subjecting the diamond film to a temperature of above about 1000.degree. C. and a hydrostatic pressure of above about 3 kilobars.
REFERENCES:
patent: 4124690 (1978-11-01), Strong et al.
patent: 4174380 (1979-11-01), Strong et al.
patent: 4181505 (1980-01-01), De Vries et al.
patent: 4296144 (1981-10-01), Maby et al.
patent: 4839195 (1989-06-01), Kitamura et al.
patent: 5110579 (1992-05-01), Anthony et al.
patent: 5371383 (1994-12-01), Miyata et al.
Graphitization of diamond at zero pressure and at a high pressure. By G. Davies and T. Evans J.J. Thomson Physical Laboratory, Berkshire, England Proc. R. Soc. Lond. A. 328 pp. 413-427 1972.
Plastic Deformation and "Work-Hardening" of Diamond. by R. C. DeVries Mat. Res. Bull. vol. 10 No. 11 pp. 1193-1200, 1975.
Anthony Thomas R.
Banholzer William F.
Spiro Clifford L.
Webb Steven W.
Williams Bradley E.
General Electric Company
King Roy V.
LandOfFree
Method for enhancing the toughness of CVD diamond does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for enhancing the toughness of CVD diamond, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for enhancing the toughness of CVD diamond will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2255285