Method for eliminating bismuth from molten lead by adding...

Specialized metallurgical processes – compositions for use therei – Processes – Free metal or alloy reductant contains magnesium

Reexamination Certificate

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

Reexamination Certificate

active

06840980

ABSTRACT:
A method for eliminating bismuth from molten lead with calcium and magnesium, in which the addition of calcium and magnesium is made in the form of lumps two Mg—Ca alloys, one containing predominantly Mg, the other containing predominantly Ca, each having a liquidus temperature lower than 650° C., and preferably lower than 600° C. A preferred treatment utilizes a first alloy containing 12-25% Ca, close to the eutectic alloy at 16.2% by weight Ca, and a second alloy containing 60-80% Ca. The method enables rapid elimination of bismuth, and adjustment of the Ca/Mg ratio during the treatment.

REFERENCES:
patent: 5041160 (1991-08-01), Zuliani et al.
patent: 343012 (1995-09-01), None
patent: 2514786 (1983-04-01), None
patent: 2764905 (1998-12-01), None
patent: 378469 (1973-04-01), None

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for eliminating bismuth from molten lead by adding... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for eliminating bismuth from molten lead by adding..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for eliminating bismuth from molten lead by adding... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3398538

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.