ABSTRACT:
Sheet cladding is applied to a substrate by applying powdered glass to the seams of the cladding after it has been assembled to the substrate. A vacuum at which the glass can be melted without decomposition is established and the glass is melted in the presence of preselected gas. Thereafter, the sheet cladding and the substrate are diffusion bonded.
REFERENCES:
patent: 3145466 (1964-08-01), Federska et al.
patent: 3904101 (1975-09-01), Beltran et al.
patent: 3952939 (1976-04-01), Schilling et al.
patent: 4043498 (1977-08-01), Conn, Jr.
patent: 4096615 (1978-01-01), Cross
patent: 4117970 (1978-10-01), Hamilton et al.
patent: 4137619 (1979-02-01), Beltran et al.
Beltran Adrian M.
Schilling William F.
General Electric Company
Gilden Leon
Squillaro Jerome C.
LandOfFree
Method for diffusion bonding sheet claddings to superalloy subst does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for diffusion bonding sheet claddings to superalloy subst, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for diffusion bonding sheet claddings to superalloy subst will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-295840