ABSTRACT:
A method for predicting the location of stress corrosion cracking in a steel gas pipeline in which in-line stress corrosion cracking smart tool data, external low level metal loss data and soil characterization data are compiled to predict the location of stress corrosion cracking in a steel gas pipeline segment.
REFERENCES:
patent: 3762446 (1973-10-01), Tungseth et al.
patent: 4241430 (1980-12-01), Kayem et al.
patent: 4507019 (1985-03-01), Thompson
patent: 4885723 (1989-12-01), Havira et al.
patent: 5323429 (1994-06-01), Roarty et al.
patent: 5526689 (1996-06-01), Coulter et al.
patent: 5571955 (1996-11-01), Beavers et al.
patent: 5587534 (1996-12-01), McColskey et al.
patent: 5728943 (1998-03-01), Colter, Jr. et al.
patent: 5883311 (1999-03-01), Hettiarachchi et al.
patent: 5883815 (1999-03-01), Drakulich et al.
patent: 6107811 (2000-08-01), Caudill et al.
patent: 6155292 (2000-12-01), Kurata
patent: 6243657 (2001-06-01), Tuck et al.
patent: 6405156 (2002-06-01), Kern et al.
Marr et al, “Procedures Guide Prediction, Evaluation of Stress Corrosion”, Corrosion and Pipe Protection, vol. 81, No. 3, Mar. 1988.
Czyz et al, “Multi-Pipeline Geographical Information System Based on High Accuracy Inertial Surveys”, Proceedings of IPC 2000 International Pipeline Conference, Oct. 2000, ASME Paper No. IPC00-138, pp. 1-5.
Leeds et al, “Modified Analysis Method Helps Coating Fault, Pipe Assessment”, Corrosion and Pipe Protection, vol. 83, No. 3, Mar. 2000.
Leis et al, “Stress-Corrosion Cracking On Gas-Transmission Pipelines History, Causes and Mitigation”, Proceedings, First International Business Conference on Onshore Pipelines, Berlin, Dec. 1997.
Budenkov et al., “Use of Rayleigh Waves in Testing Stress-Corrosion Breaks in Pipelines by the Acoustic Emission Method”. p. 71-78. Oct. 2000. Izhevsk State Tech Unvi. Russia.
Evertz et al., “Test Method for the Investigation of the Susceptibility to Cracking in Near Neutral pH Solution” 1999 Steel-Research p. 183-187.
Bracewell & Giuliani LLP
Kinder Morgan, Inc.
Rodriguez Paul L.
Stevens Thomas H.
LandOfFree
Method for detecting near neutral/low pH stress corrosion... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for detecting near neutral/low pH stress corrosion..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for detecting near neutral/low pH stress corrosion... will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-3548905