ABSTRACT:
Crosslinking polysilastyrene by mixing polysilastyrene with 2-15 weight % dicumyl peroxide and heating at 80.degree. C. to 500.degree. C. for 5 minutes to 5 days to produce crosslinking.

REFERENCES:
patent: 3546156 (1970-12-01), Baronnier et al.
patent: 3876605 (1975-04-01), Itoh et al.
patent: 4310651 (1982-01-01), Baney et al.
patent: 4324901 (1982-04-01), West et al.
L. D. David, "New Polysilane Polymers: Polysilastyrene and Polyphenylmethylisilylene," University Wisconsin--Madison 1981.
Chapter 19 by Robert West entitled "Polysilane Precursors to Silicon Carbide."

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for crosslinking of polysilastyrene does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for crosslinking of polysilastyrene, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for crosslinking of polysilastyrene will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1366399

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.