ABSTRACT:
A method for the continuous recovery of non-iron metals from a molten metallurgical slag containing lead, copper or nickel by continuously reducing the layer with carbon dust. The metal layer produced at the furnace bottom is maintained sufficiently thin so that it is between 0 and 20 mm thick. Injection of carbon dust into the metal layer is avoided.

REFERENCES:
patent: 3579328 (1971-05-01), Aas
patent: 3585024 (1971-06-01), Cenerazzo
patent: 4032327 (1977-06-01), Donaldson
patent: 4110107 (1978-08-01), Paulson

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for continuous reduction of molten metallurical slag in a does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for continuous reduction of molten metallurical slag in a, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for continuous reduction of molten metallurical slag in a will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1427391

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.