Method for connecting superalloy components

Metal treatment – Compositions – Heat treating

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

148 115Q, 148127, C22F 110

Patent

active

047509465

ABSTRACT:
Components (5) in a superalloy, in particular a dispersion hardened nickel based alloy, are connected together by pressure bonding in the solid condition with the greatest possible limitation of the overall deformation of the complete components (5) by lateral restraint (7), the actual bonding zone (6) having short-term intensive dynamic plastic flow imposed on it and, taking account of the deformation temperature, the local deformation rate .epsilon..sub.l and the local deformation .epsilon..sub.l referred to the bonding zone (6) are matched together in such a way that the driving force during the subsequent heat treatment of the complete workpiece above the recrystallization temperature is sufficient to force the formation of coarse grain under all conditions. It can then be assumed that, in general, the expression ##EQU1## h.sub.o =height of the bonding zone (6) before connection, h.sub.f =height of the bonding zone (6) after connection,

REFERENCES:
patent: 4490186 (1984-12-01), Sines et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for connecting superalloy components does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for connecting superalloy components, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for connecting superalloy components will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-503057

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.