ABSTRACT:
Delayed petroleum coke is calcined in an internally-fired vertical shaft kiln. A downwardly-moving bed of green coke is preheated in the top of the kiln by rising combustion gases, then heat soaked at calcining temperatures in the intermediate section of the kiln, and finally cooled by recycle gas moving upwardly from the lower part of the kiln. Partially cooled calcined coke is recovered from the bottom of the kiln.

REFERENCES:
patent: 1671673 (1928-05-01), Doerschuk et al.
patent: 2716628 (1955-08-01), Weikart
patent: 2738316 (1956-03-01), Metrailer
patent: 2757129 (1956-07-01), Reeves et al.
patent: 2796390 (1957-06-01), Elliott
patent: 2982701 (1961-05-01), Scott, Jr.
patent: 3086923 (1963-04-01), Destremps et al.
patent: 3173852 (1965-03-01), Smith
patent: 3823073 (1974-07-01), Minkkinen
patent: 4066420 (1978-01-01), Danguillier et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for calcining delayed coke does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for calcining delayed coke, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for calcining delayed coke will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2261009

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.