ABSTRACT:
A powder mixture for applying gas phase aluminide coatings to nickel or cobalt base superalloys is described. A preferred mixture consists essentially of Co.sub.2 Al.sub.5, NH.sub.4 F.HF, and chromium metal. The mixture is substantially free of aluminum oxide.

REFERENCES:
patent: 3079276 (1963-02-01), Puyear et al.
patent: 3257230 (1966-06-01), Wachtell et al.
patent: 3276903 (1966-10-01), Galmiche
patent: 3667985 (1972-06-01), Levine et al.
patent: 3801353 (1974-04-01), Brill-Edwards
patent: 3837901 (1974-09-01), Seybolt
patent: 3904789 (1975-09-01), Spiers
patent: 3958047 (1976-05-01), Baldi
patent: 4132816 (1979-02-01), Benden et al.
patent: 4142023 (1979-02-01), Bornstein et al.
patent: 4148275 (1979-04-01), Benden et al.
patent: 4293338 (1981-10-01), Rose
patent: 4332843 (1982-06-01), Ahuja
G. W. Goward et al, "Formation and Degradation Mechanisms of Aluminide Coatings on Nickel-Base Superalloys," Transactions of the ASM, vol. 60, 1967, pp. 228-241.
K. Godlewski et al, "Effect of Chromium on the Protective Properties of Aluminide Coatings," Oxidation of Metals, vol. 26, Nos. 1/2, 1986, pp. 125-138.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for applying aluminide coatings to superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for applying aluminide coatings to superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for applying aluminide coatings to superalloys will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1932556

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.