ABSTRACT:
Bismuth is added to molten steel in a ladle, and the molten steel is covered with a slag layer sufficiently thick to prevent a decrease in the bismuth content during the time the molten steel is in the ladle.
REFERENCES:
patent: 3516821 (1970-06-01), Neu
patent: 3673004 (1972-06-01), Dumitrescu
patent: 3762915 (1973-10-01), Heine
patent: 4244737 (1981-01-01), Holowaty
patent: 4247326 (1981-01-01), Quinto
patent: 4255188 (1981-03-01), Riekels
Lazaridis Nassos A.
O'Neil Robert D.
Pielet Howard M.
Inland Steel Company
Rosenberg Peter D.
LandOfFree
Method for adding bismuth to steel in a ladle does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for adding bismuth to steel in a ladle, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for adding bismuth to steel in a ladle will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1562340