ABSTRACT:
Internal structure of a metal strip is monitored by applying cyclically varying magnetic flux to the strip and sensing the flux induced in the strip. Signals corresponding to the magnetic field intensity of the applied cyclically varying field and to the resulting induced flux indicate the loss of energy due to the internal structure of the strip. Making a similar determination by similar monitoring apparatus following annealing of the strip allows the effect of the annealing to be determined. The signals from the two monitoring apparatus can be used to generate a comparison signal to control the operation of the annealing treatment apparatus.
REFERENCES:
patent: 2059054 (1936-10-01), Stargardter
patent: 2211017 (1940-08-01), Leifer et al.
patent: 2534420 (1950-12-01), Delaney
patent: 2828467 (1958-03-01), Stauffer
patent: 3130363 (1964-04-01), Camp et al.
patent: 3281678 (1966-10-01), Cilyo
patent: 3723859 (1973-03-01), Leonard
Siemens Aktiengesellschaft
Skiff Peter K.
LandOfFree
Method and device for the continuous, contactless monitoring of does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method and device for the continuous, contactless monitoring of , we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method and device for the continuous, contactless monitoring of will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-749864