ABSTRACT:
Methods of forming a conversion coating on metal surfaces such as galvanized steel are provided. The methods comprise reacting the metal surface with an aqueous solution of a water soluble polyacrylic acid or homopolymer thereof, maleic or acrylic acid/allyl ether copolymer alone or with an acid.
REFERENCES:
patent: 3468724 (1969-09-01), Reinhold
patent: 3682713 (1972-08-01), Ries et al.
patent: 4136073 (1979-01-01), Muro et al.
patent: B14191596 (1990-06-01), Dollman et al.
patent: 4273592 (1981-06-01), Kelly
patent: 4294627 (1981-10-01), Heyes
patent: 4370177 (1983-01-01), Frelin et al.
patent: 4422886 (1983-12-01), Das et al.
patent: 4471100 (1984-09-01), Tsubakimoto et al.
patent: 4500693 (1985-02-01), Takehara et al.
patent: 4709091 (1987-11-01), Fukumoto et al.
patent: 4847410 (1989-07-01), Lickei et al.
patent: 4861429 (1989-08-01), Barnett et al.
patent: 4872995 (1989-10-01), Chen et al.
patent: 4895622 (1990-01-01), Barnett et al.
patent: 4913822 (1990-04-01), Chen et al.
patent: 4921552 (1990-05-01), Sander et al.
patent: 4929362 (1990-05-01), Chen
patent: 4959156 (1990-09-01), Lickei et al.
patent: 5158622 (1992-10-01), Reichgott
Chem.Abstract 11:10119V, 1989.
Chen Fu
Reichgott David W.
Betz Laboratories Inc.
Boyd Steven D.
Ricci Alexander D.
Silverberg Sam
LandOfFree
Method and composition for treatment of galvanized steel does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method and composition for treatment of galvanized steel, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method and composition for treatment of galvanized steel will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-576947