ABSTRACT:
A method is provided for improving the electrical characteristics of grain-oriented silicon steel sheet by heating the steel to temperatures above 1000.degree. F. and then deforming grooves to refine the magnetic domains, optionally, post heat treating to form fine recrystallized grains in the vicinity of the hot deformations, preferably using protrusions on a scribing roll as the sheet moves between a scribing roll and a back-up anvil roll at deforming pressures range up to 120,000 pounds per square inch.

REFERENCES:
patent: 4711113 (1987-12-01), Benford
patent: 4742706 (1988-05-01), Sasaki et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method and apparatus for refining the domain structure of electr does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method and apparatus for refining the domain structure of electr, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method and apparatus for refining the domain structure of electr will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-535930

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.