ABSTRACT:
An ultrasonic defect detection apparatus comprising a supersonic probe, a rotary shaft for revolving the probe along the inner surface of a pipe to be examined, and a hollow shaft removably connected to the rotary shaft for vertically moving the probe. Water acting as a contact medium is circulated between the operating surface of the probe and a water tank through the rotary shaft and the hollow shaft. The apparatus is inserted into a pipe to be examined such as the control rod housing of an atomic reactor through the bottom opening of the pipe, and can be operated from a remote place for the sake of safety.

REFERENCES:
patent: 3002375 (1961-10-01), Moffatt et al.
patent: 3960006 (1976-06-01), Smith

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method and apparatus for examining weld defects in vertical pipe does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method and apparatus for examining weld defects in vertical pipe, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method and apparatus for examining weld defects in vertical pipe will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2298984

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.