ABSTRACT:
A metalworking die has a soft metal plating on its contact surfaces. The plating produces a continuous lubricant supply which is only depleted slowly when employed in a hot metalworking operation. In forming a near-net-shape part using this die, the metalworking piece is coated with a glass lubricant. A temporary lubricant of graphite is also sprayed on the coated die.
REFERENCES:
patent: 3360157 (1967-12-01), Bolt et al.
patent: 3655349 (1972-04-01), Shah et al.
patent: 4040282 (1977-08-01), Saunders
patent: 4074922 (1978-02-01), Murdoch
patent: 4095449 (1978-06-01), Roach et al.
patent: 4571983 (1986-02-01), Sanborn et al.
patent: 4595473 (1986-06-01), Kalamasz
patent: 4621026 (1986-11-01), Robinson
patent: 4787228 (1988-11-01), Weisner et al.
Butler Rodney
General Electric Company
Hail III Joseph J.
Snyder Marvin
Stoner Douglas E.
LandOfFree
Metalworking dies with soft metal lubricant platings does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Metalworking dies with soft metal lubricant platings, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Metalworking dies with soft metal lubricant platings will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2266562