ABSTRACT:
A method of processing an impure aluminum base alloy containing a substantial amount of silicon and a deleterious amount of titanium, which includes melting the alloy and stirring the molten alloy with a molten fluoride flux less dense than the alloy and having a boiling point above the alloy's liquidus temperature, then permitting the stirred mixture to stand to settle out a molten alloy in which the titanium content is reduced but not entirely eliminated, and separating the settled out alloy from the flux.
REFERENCES:
patent: 2930676 (1960-03-01), Byrns
patent: 2974032 (1961-03-01), Grunert et al.
patent: 3083093 (1963-03-01), Grunert
patent: 3198625 (1965-08-01), Stroup
Andrews M. J.
Ethyl Corporation
Johnson Donald L.
Leonard Paul H.
Sieberth John F.
LandOfFree
Metallurgical process for purifying aluminum-silicon alloy does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Metallurgical process for purifying aluminum-silicon alloy, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Metallurgical process for purifying aluminum-silicon alloy will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-902051